🔩 Fix it like a pro, bond it like a boss!
Super Alloy 1 Mixed Diameter Sample offers a versatile welding solution with four rods in two diameters and 1 oz of liquid flux. Designed to work at 350°F, it prevents warpage and metal damage while delivering an impressive 20,000 psi bond strength. Perfect for bonding dissimilar metals such as brass, aluminum, copper, and stainless steel, it supports a wide range of heat sources including propane, MAPP gas, and soldering irons, making it the go-to choice for professional-grade metal repairs.







| ASIN | B0CDQTL9MF |
| Best Sellers Rank | #57,714 in Industrial & Scientific ( See Top 100 in Industrial & Scientific ) #167 in Solder #274 in Soldering Parts & Accessories #1,280 in Welding Equipment & Accessories |
| Brand | Muggy Weld |
| Brand Name | Muggy Weld |
| Color | Black |
| Customer Reviews | 4.2 out of 5 stars 31 Reviews |
| Item Weight | 0.75 Pounds |
| Manufacturer | Muggy Weld |
| Manufacturer Part Number | 046728984727 |
| Material | Metal |
| Material Type | Metal |
| UPC | 046728984727 |
| Unit Count | 1.0 Count |
P**L
Super Easy to Use
Wow, funny name but this stuff really works awesome! I had a highly cosmetic zinc investment casting for a point of purchase display that went wrong and I was able to 100% fix the issue and save the parts! Super easy to use. Blends with the zinc so well that I can't even find the places I fixed to be able to brag about it! Stunning results in seconds! I wish it came in smaller diameter tho. Going to run these thru a pull plate to get them down to a size suitable for my work piece without so much waste
Y**R
Ez peazy
Had a pin hole leak in a pewter Dragon flask. Using a 25 watt soldering iron, fluxing both iron and around the hole in the flask. I gathered a bead of the alloy onto the iron, and placed it over the hole. Held it there until flux changed colour. Alloy flowed, patch complete. Filed down and you can hardly tell the flask has a patch.
B**P
Doesn't work
Had high hopes for this product but it just doesn't work. Won't stick to material regardless of how you prep, heat, flux, etc. Followed instructions but it was no use. Don't waste your time or money on this stuff.
A**R
good stuff
I was trying to secure galvanized pipe I bought to ordinary steel plate. I used the enclosed flux to wet the surface of the steel plate and coated it using a torch with 50/50 solder. Then I coated the galvanized pipe with the same flux and heated it. Put a tin coat of super alloy 1 solder on it and mixed it with the 50/50 solder. Seemed to secure it well.
R**N
Works as advertised
Wonderful product... will be purchasing more
H**A
Expensive- low melting point
Expensive, long delivery time, didn’t quite work in my hands for brazing… probably needed TIG for my project. Your mileage may vary
R**E
Weld
Works as advertised. With a little practice, all is ggod.
D**S
That the solder filled the gap.
I really liked the product.i bought a scraper for cutting out the inside of boxes made on a wood lathe.it didn't come with a handle,so I made a handle on the lathe.i molded a piece of brass to fit around the metal tang.it wasn't closed all the way,and it keep the handle from splitting,so there ya go i used the muggy weld and sealed the brass together wonderful job.
Trustpilot
2 days ago
2 weeks ago